Por favor, use este identificador para citar o enlazar este ítem: http://dspace.espoch.edu.ec/handle/123456789/20214
Registro completo de metadatos
Campo DC Valor Lengua/Idioma
dc.contributor.advisorTubón Usca, Gabriela Viviana-
dc.contributor.authorEstrada Cajamarca, Paola Alejandra-
dc.date.accessioned2024-03-06T20:04:54Z-
dc.date.available2024-03-06T20:04:54Z-
dc.date.issued2022-10-24-
dc.identifier.citationEstrada Cajamarca, Paola Alejandra. (2022). Síntesis y caracterización de nanocelulosa a partir de residuos de biomasa de cáscaras de piña, tusa de maíz, colillas de cigarrillo y papel reciclado. Escuela Superior Politécnica de Chimborazo. Riobambaes_ES
dc.identifier.urihttp://dspace.espoch.edu.ec/handle/123456789/20214-
dc.descriptionEl objetivo de la presente investigación fue obtener nanocelulosa a partir de residuos de biomasa de cáscaras de piña, tusa de maíz, colillas de cigarrillo y papel reciclado, mediante un estudio teórico práctico con base a procesos fisicoquímicos. Se inició con la caracterización de los residuos que actuaron como materia prima para el procedimiento, determinando el porcentaje de humedad, cenizas, densidad, solubilidad en agua caliente, lignina y alfa celulosa; además, la materia prima, celulosa y nanocelulosa se analizó a través del microscopio óptico, espectroscopia infrarroja (FTIR), microscopia electrónica de barrido (SEM) y espectrofotómetro UV Visible. El proceso comenzó con la realización de un pretratamiento por cada materia prima, posteriormente se extrajo celulosa con tres repeticiones por tratamiento alcalino con hidróxido de sodio (NaOH) al 5% a dos temperaturas (50°C ; 90°C), en el caso de la cáscara de piña se añadió ácido acético (CH3COOH) en relación 3:1, para obtener una celulosa blanquecina se empleó hipoclorito de sodio (NaClO) al 1%, se interpretó los resultados mediante un análisis estadístico ANOVA, considerando que el tratamiento del papel reciclado obtuvo el mejor rendimiento (89,19% a 50°C). Finalmente se sintetizó nanocelulosa aplicando el proceso de hidrolisis ácida donde se utilizó ácido sulfúrico (H2SO4) al 65%, a 45°C, adicionando ultrasonido. Se concluye que las muestras de nanocelulosa poseen una transmitancia entre 1,826 y 93,878%, presenta medidas específicas que varían entre 50nm a 9um identificadas a partir del SEM, se observó los grupos funcionales que presenta la celulosa empleando FTIR y el EDS demostró que la composición está dada por carbono y oxígeno. Se recomienda realizar un mejor pretratamiento para eliminar impurezas y así evitar que la celulosa se compacte; respecto a la nanocelulosa para su caracterización realizar láminas con un espesor favorable y diluciones apropiadas.es_ES
dc.description.abstractThe research objective was to obtain nanocellulose from biomass residues of pineapple peels, corn husks, cigarette butts and recycled paper, by means of a theoretical and practical study based on physicochemical processes. It began with the characterization of the residues that acted as raw material for the procedure, determining the percentage of moisture, ash, density, solubility in hot water, lignin and alpha cellulose; in addition, the raw material, cellulose and nanocellulose were analyzed by optical microscopy, infrared spectroscopy (FTIR), scanning electron microscopy (SEM) and UV Visible spectrophotometer. The process began with the implementation of a pretreatment for each raw material, then cellulose was extracted with three replicates by alkaline treatment with 5% sodium hydroxide (NaOH) at two temperatures (50°C; 90°C), in the case of pineapple peel acetic acid (CH3COOH) was added at a ratio of 3: 1, to obtain a whitish cellulose 1% sodium hypochlorite (NaClO) was used, the results were interpreted by ANOVA statistical analysis, considering that the recycled paper treatment obtained the best yield (89.19% at 50°C). Finally, nanocellulose was synthesized by applying the acid hydrolysis process using 65% sulfuric acid (H2SO4), at 45°C, with the addition of ultrasound. It is concluded that the nanocellulose samples have a transmittance between 1.826 and 93.878%, it presents specific measurements that vary between 50nm to 9um identified from the SEM, the functional groups that cellulose presents were observed using FTIR and the EDS showed that the composition is given by carbon and oxygen. It is recommended to carry out a better pretreatment to eliminate impurities and thus prevent the cellulose from compacting; with respect to the nanocellulose for its characterization, to make sheets with a favorable thickness and appropriate dilutions.es_ES
dc.language.isospaes_ES
dc.publisherEscuela Superior Politécnica de Chimborazoes_ES
dc.relation.ispartofseriesUDCTFC;96T00820-
dc.rightsinfo:eu-repo/semantics/openAccesses_ES
dc.subjectCÁSCARAS DE PIÑAes_ES
dc.subjectTUSAS DE MAÍZes_ES
dc.subjectCOLILLAS DE CIGARRILLOes_ES
dc.subjectPAPEL RECICLADOes_ES
dc.subjectTRATAMIENTO ALCALINOes_ES
dc.subjectCELULOSAes_ES
dc.subjectHIDRÓLISIS ÁCIDAes_ES
dc.subjectNANOCELULOSAes_ES
dc.titleSíntesis y caracterización de nancelulosa a partir de residuos de biomasa de cáscaras de piña, tusa de maíz, colillas de cigarrillo y papel reciclado es_ES
dc.typeinfo:eu-repo/semantics/bachelorThesises_ES
dc.contributor.miembrotribunalLinda Mariuxi Flores Fiallos-
dc.rights.urihttps://creativecommons.org/licenses/by-nc-sa/3.0/ec/es_ES
Aparece en las colecciones: Ingeniero/a Químico/a

Ficheros en este ítem:
Fichero Descripción Tamaño Formato  
96T00820.pdf7,21 MBAdobe PDFVista previa
Visualizar/Abrir


Este ítem está sujeto a una licencia Creative Commons Licencia Creative Commons Creative Commons